BS EN ISO 15614-11:2002 – Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 11: Electron and laser beam welding

1 Scope
This European Standard specifies how a welding procedure specification for electron or laser beam welding is qualified by a welding procedure test.
This standard is a part of a series of standards, details of this series are given in prEN ISO 15607, annex A.
It defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of variables listed in clause 8.
Tests shall be carried out in accordance with this standard together with additional tests when specified.
This standard applies to metallic materials, irrespective of the shape of the parts, their thicknesses, manufacturing method (rolling, forging, casting, sintering, etc.) and their heat treatment. It covers unlimitedly the production of new parts and repair work.
2 Normative references
This European Standard incorporates by dated or undated reference, provisions from other publications. These normative references are cited at the appropriate places in the text and the publications are listed hereafter. For dated references, subsequent amendments to or revisions of any of these publications apply to this European Standard only when incorporated in it by amendment or revision. For undated references the latest edition of the publication referred to applies (including amendments).
EN 571-1, Non destructive testing — Penetrant testing — Part 1 : General principles.
EN 895, Destructive tests on welds in metallic materials — Transverse tensile test.
EN 910, Destructive tests on welds in metallic materials — Bend tests.
EN 970, Non-destructive examination of fusion welds — Visual examination.
EN 1043-2, Destructive test on welds in metallic materials — Hardness test — Part 2: Micro hardness testing on welded joints.
EN 1290, Non-destructive examination of welds — Magnetic particle examination of welds.
EN 1321, Destructive tests on welds in metallic materials — Macroscopic and microscopic examination of welds.
EN 1435, Non-destructive examination of welds — Radiographic examination of welded joints.
EN 1714, Non destructive examination of welds —- Ultrasonic examination of welded joints.
EN ISO 6947, Welds — Working positions — Definitions of angles of slope and rotation (ISO 6947:1993).
prEN ISO 15607, Specification and approval of welding procedures for metallic materials – General rules (ISO/DIS 15607:2000).
prEN ISO 15609-3:2000,Specification and approval of welding procedures for metallic materials – Welding procedure specification — Part 3: Electron beam welding (ISO/DIS 15609-3:2000).
prEN ISO 15609-4:2000, Specification and approval of welding procedures for metallic materials – Welding procedure specification — Part 4: Laser beam welding (ISO/DIS 15609-4:2000).
EN ISO 13919-1, Welding — Electrons and laser beam welded joints — Guidance on quality levels for imperfections — Part 1: Steel (ISO 13919-1:1996).
prEN ISO 13919-2, Welding — Electron and laser beam welded joints — Guidance on quality levels for imperfections — Part 2: Aluminium and its weldable alloys (ISO/FDIS 13919-2:1999).
BS EN ISO 15614-11:2002 – Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 11: Electron and laser beam welding